Wea are making our first ceramic calls. What do most of you use to condition the surface? I want to do it right the first time.
Mike
I really appreciate your help on this one!
-
Nothing to start, then as the surface gets clogged with striker bits I use a Scotchbrite and maybe some alcohol to clean it.
-
Nothing to start, then as the surface gets clogged with striker bits I use a Scotchbrite and maybe some alcohol to clean it.
Thanks Ed, I assumed something like that I had hoped you would answer! Thanks my friend. I like the sound just as it is.
Mike